by 78spyder » Wed Nov 26, 2008 12:36 am
I'm going to be hitting the door panals, I see Sems, VHT and Krylon Fusion all make a plastic coating product. VHT makes a dye and a paint. I've had good luck with both VHT and Sems products, and I have some yet to be installed rear quarter window fins that I used the fusion on and they look great, but I wont know how durable they are for awhile. I'm thinking about going with the VHT paint. Can anyone give any feedback? Yes, I am a nut about preparation, so it will get several soap/water and solvent baths prior to spraying and possibly a coat of adhesion promoter for good measure.